Resources
Frequently Asked Questions
RESCOBOND AA-22S
-
Do Rescobond AA-22S linings need to be dried after air setting to resist shipping damage?
-
Will undried Rescobond AA-22S absorb moisture from the air like plastics do?
-
Will freeze/thaw cycles affect unheated Rescobond AA-22S installations?
-
Must the undried Rescobond AA-22S linings be kept dry after air setting?
-
Must the Rescobond AA-22S lining be dried if it is going to be stored before use?
-
Is unheated Rescobond AA-22S affected by steam which is sometimes used as part of the start-up process?
-
An installation is going to be hydrostatically tested. What precautions must be taken with Rescobond AA-22S?
CASTABLE
MONOLITHICS
What is the best practice to install monolithic products in cold weather?
Question :
What is the best practice to install monolithic products in cold weather?
During cold weather, the refractory lining and the applied surface should be kept at a temperature above 50°F (10°C) during application, curing, and right before the start of the dryout/heatup procedure. Cement bonded castable must not be exposed to freezing temperature (below 32°F / 0°C) during the installation and initial curing phases). If exposed to freezing temperatures during storage, dry monolithic products should be heated to a temperature between 50°F (10°C) and 80°F (27°C) prior to installation for best results. Measure material temperature for best results. An immersion thermometer is a good method to measure the refractory monolithic temperature